MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

EMS-Grivory Grilamid® TR 30 LS nat Nylon 6I/X, Flame Retardant, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Flame Retardant; Lubricant

Features: Aromatic; Barrier Resin; Flame Retardant; Food Contact Acceptable; Hydrolysis Resistant; Lubricated

Uses: Appliance Components; Automotive Applications; Automotive Electronics; Automotive Interior Parts; Cell Phone; Connectors; Containers; Electrical/Electronic Applications; Lighting Applications; Medical/Healthcare Applications; Pneumatic Applications

Agency Ratings: EU Food Contact; FDA Food Contact

Forms: Granules

Processing Method: Injection Stretch Blow Molding; Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Water Absorption 3.5 %3.5 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 9.0 %9.0 %ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 59.4 µm/m-°C33.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 59.4 µm/m-°C33.0 µin/in-°FISO 11359-2
Maximum Service Temperature, Air 100 °C212 °FLong Term; ISO 2578
 120 °C248 °FShort Term
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FUnannealed; ISO 75-2/A
Minimum Service Temperature, Air 80.0 °C176 °FLong Term; ISO 2578
Glass Transition Temp, Tg 160 °C320 °F10ºC/min; ISO 11357-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM192 / 307551

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.