MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Zotefoams Plastazote® LD50CN Conductive Low Density Polyethylene Foam
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Compliant with EC food contact and US FDA regulations.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0500 g/ccNominal skin/skin; BS ISO 7214 1998
 0.0430 - 0.0580 g/ccsheet density
Cell Length 0.600 - 1.10 mm
 0.850 mmTypical Diameter
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 7310 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.515 MPaISO 7214 1998
Elongation at Break 65 %
Compressive Yield Strength 0.120 MPa
@Strain 10 %
BS ISO 7214 1998
 0.139 MPa
@Strain 25 %
BS ISO 7214 1998
 0.172 MPa
@Strain 40 %
BS ISO 7214 1998
 0.214 MPa
@Strain 50 %
BS ISO 7214 1998
Tear Strength 0.800 kN/mBS EN ISO 8067 1995
Compression Set 3.5 %
@Time 79200 sec,
Strain 25 %
24 hr recovery; BS ISO 7214 1998
 7.5 %
@Time 79200 sec,
Strain 25 %
0.5 hr recovery; BS ISO 7214 1998
 10 %
@Time 79200 sec,
Strain 50 %
24 hr recovery; BS ISO 7214 1998
 16 %
@Time 79200 sec,
Strain 50 %
0.5 hr recovery; BS ISO 7214 1998
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 ohm-cmASTM D991-89
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0420 W/m-Kmean temp of 10°C; ISO 8302 1991
Maximum Service Temperature, Air 105 °C
Minimum Service Temperature, Air -70.0 °C
Flammability Test 0.70
@Thickness 13.0 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 1.0
@Thickness 5.00 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zotefoams Plastazote® LD32CN Conductive Low Density Polyethylene Foam
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam
Zotefoams Plastazote® LD29 Low Density Polyethylene Foam
Zotefoams Plastazote® LD24MC Low Density Polyethylene Foam, Medium Cell
Zotefoams Plastazote® LD24LC Low Density Polyethylene Foam, Large Cell

PZOTEF921 / 150677

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.