MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akrochem Lowilite™ 77UV Stabilizer
Categories: Other Engineering Material

Material Notes: Product Description: Lowilite™ 77 UV stabilizer is a highly effective light stabilizer belonging to the Hindered Amine Light Stabilizer (HALS) family of stabilizers.

Applications: Lowilite™ 77 UV stabilizer as a stabilizer is superior to classic products such as UVAs and nickel containing stabilizers. Lowilite™ 77 UV stabilizer is very suitable, alone or in combination with oligemeric HALS, for the UV stabilization of tapes and thick items such as car bumpers and garden furniture. Lowilite™ 77 UV stabilizer is recommended for polymers such as polyolefins, PS, HIPS, ABS, SAN and ASA. It is also effective in polyurethanes, polyamides and polyacetals.

CAS No: 52829-07-9

EINECS: 258-207-9

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.560 g/cc0.0202 lb/in³
Molecular Weight 481 g/mol481 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 80.0 - 85.0 °C176 - 185 °F
 
Descriptive Properties
AppearanceSlightly yellow micropellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH542 / 315460

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.