MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® VESPEL PI SP211 PI + 15% graphite + 10% PTFE
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled; Thermoplastic Polyimide, Molded, PTFE Filled

Material Notes: The addition of 15% graphite and 10% PTFE gives rise to the lowest coefficient of friction of all PI types along with the lowest wear. This type is suitable for applications where low friction and wear properties are required at temperatures of up to +150 °C.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psiASTM D 1708
Elongation at Break 3.5 %3.5 %ASTM D 1708
Modulus of Elasticity 3.10 GPa450 ksiASTM D 790
Coefficient of Friction 0.200.20p=0.05 N/mm2, v=0.6 m/s, against hardened and polished steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
30.0 µin/in-°F
@Temperature 73.4 - 140 °F
Thermal Conductivity 0.760 W/m-K5.27 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 300 °C572 °Flong term
 360 °C680 °Fshort term
Flammability, UL94 V-0V-0
 
Descriptive Properties
Coloranthracite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP073 / 250571

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.