OKULEN® 1000 – AST – black – FN9200 is an ultra high molecular low pressure polyethylene UHMW-PE with a molecular weight 5.000.000. This material properties that make it extremely versatile; the material is ideally suited for mechanical engineering – OKULEN® 1000 parts are used especially in plant construction and handling technology. The product fulfills the requirements of the ATEX – Directive for values of resistivity. It was tested on representative samples by the TUV – Nord (Germany) Properties: Conductive/Antistatic reduced; ATEX - conform; TUV approved; UV - stabilized; EU 1935/2004 & 10/2011 – conform; FDA – conform Color: black FN9200/similar RAL 9005 Range of applications: Mechanical engineering; Conveying industry; Explosion-proof zones Information provided by Okulen |