MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ LUBRICOMP™ Compound RFP36L Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP LUBRICOMP RFP36L compound is based on Nylon 6/6 resin containing 30% glass fiber, 15% PTFE/silicone. Added features of this grade include: Low Extractable, Wear Resistant.

Features: Low Extractable,Wear resistant,Food Contact Acceptable,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D792
Density 1.435 g/cc0.05184 lb/in³ASTM D792
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
 0.470 %0.470 %23°C / 50% RH; ISO 62
 0.690 %0.690 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 150 MPa21800 psi5 mm/min; ASTM D638
 150 MPa21800 psi5 mm/min; ISO 527
Elongation at Break 2.3 %2.3 %5 mm/min; ASTM D638
 2.4 %2.4 %5 mm/min; ISO 527
Tensile Modulus 10.22 GPa1482 ksi5 mm/min; ASTM D638
 10.31 GPa1495 ksi1 mm/min; ISO 527
Flexural Strength 214 MPa31000 psiISO 178
 219 MPa31800 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.14 GPa1330 ksi2 mm/min; ISO 178
 9.66 GPa1400 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 100 J73.8 ft-lbASTM D256
Izod Impact, Unnotched 7.48 J/cm14.0 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 52.0 kJ/m²24.7 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 7.00 J5.16 ft-lbASTM D3763
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.520.52ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.500.50ASTM D3702 Modified: Manual
K (wear) Factor 6.04 x 10-8 mm³/N-M3.00 x 10-10 in³-min/ft-lb-hrRing; ASTM D3702 Modified: Manual
 54.4 x 10-8 mm³/N-M27.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
13.9 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 56.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 259 °C498 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 261 °C
@Thickness 3.20 mm
502 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 253 °C
@Thickness 3.20 mm
487 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 280 - 295 °C536 - 563 °F
Zone 3 295 - 305 °C563 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 95.0 - 110 °C203 - 230 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81012 / 288959

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.