MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici RADILON® A RV500 100 NT Nylon 66, 50% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Description: PA66 50% glass fiber reinforced injection molding grade. Natural color. Suitable for parts requiring very high stiffness and high mechanical resistance, as in case of metal replacement applications.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Industries: Automotive, Consumer Industry Goods

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183
Water Absorption 4.6 %
@Thickness 2.00 mm
4.6 %
@Thickness 0.0787 in
Immersion at 23°C; ISO 62
Moisture Absorption 1.10 %
@Thickness 2.00 mm
1.10 %
@Thickness 0.0787 in
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inMelt Temp/Mold Temp/Cavity Pressure: 300/90/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inMelt Temp/Mold Temp/Cavity Pressure: 300/90/60; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 175 MPa25400 psi5mm/min; ISO 527-2/1A
Tensile Stress  50.0 MPa
@Strain 0.2 %
7250 psi
@Strain 0.2 %
Break
 128 MPa
@Strain 3 %
18600 psi
@Strain 3 %
Break
 150 MPa
@Strain 1.95 %
21800 psi
@Strain 1.95 %
Break
Elongation at Break 3.5 %3.5 %5mm/min; ISO 527-2/1A
Tensile Modulus 12.5 GPa1810 ksi1mm/min; ISO 527-2/1A
Secant Modulus  5.50 GPa
@Strain 3 %
798 ksi
@Strain 3 %
Break
 12.5 GPa
@Strain 0.25 %
1810 ksi
@Strain 0.25 %
Break
 16.0 GPa
@Strain 0.0 %
2320 ksi
@Strain 0.0 %
Break
Charpy Impact Unnotched 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.80 J/cm²
@Temperature 23.0 °C
13.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohm500V; IEC 60093
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 305 °C554 - 581 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI154 / 313655

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.