MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hexcel® LC1000 Liquid Crystal Polymer for RF Interference Control
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Description:
  • Dielectric absorber based on a Liquid Crystal Polymer (LCP) thermoplastic.
  • Can be injection molded into custom shapes, provides good high temperature performance and has the ability to flow into thin-walled parts.
  • Typical applications include electrical connectors, housings, and circuit covers.
  • Ideal for applications in the 10+ GHz range, but can be tailored to specific requirements.
  • Halogen free, RoHS and REACH compliant.
  • Flammability rating is UL-94 V0.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84.0ASTM D2240
Tensile Strength 18.8 ksiASTM D638
Elongation at Break 6.00 %ASTM D638
Tensile Modulus 450 ksiASTM D638
Flexural Strength 265 ksiat failure; ASTM D790
Flexural Modulus 887 ksiASTM D790
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.10e+10 ohmASTM D257
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9591 / 322745

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.