MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Lanxess Uniplex 260 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex 260 is a solid polyol benzoate plasticizer, processing aid and modifier for a wide range of polymers, including polyester, acrylic resins, polyvinyl acetate, cellophane and nitrocellulose. Uniplex 260 is especially recommend for use in heat seal applications and coatings.

Chemical composition: Glyceryl Tribenzoate

General Uniplex 260 is a solid polyol benzoate plasticizer, processing aid and modifier for a wide range of polymers, including polyester, acrylic resins, polyvinyl acetate, cellophane and nitrocellulose. Uniplex 260 is especially recommend for use in heat seal applications and coatings.

Applications: Uniplex 260 is used as a heat-activatable plasticizer hot melt adhesives based on polyester, acrylic resins and polyvinyl acetate. The adhesion promoting plasticizer improves the heat seal properties of cellophane and nitrocellulose coatings. Uniplex 260 is particularly suitable for use in hot melt adhesives. When used in polyvinyl acetate-based adhesives it must be ensured that the temperature of mixing and processing up to the end use bonding remains below the melting point of the product; melting of Uniplex 260 results in an essentially irreversible tackifying and plasticizing of the coating. Typically, a high shear mixer is used to reduce the particle size of the Uniplex 260 formulation until a smooth stable dispersion is obtained. Uniplex 260 may be incorporated at levels of 20 to 40 parts based on 100 parts polymer. Uniplex 260 may be used in cellophane coatings to improve heat-seal properties, without affecting color and clarity of the film. Uniplex 260 an outstanding plasticizer for nitrocellulose coatings, lacquers and films where it promotes heat-sealability and adhesion, and creates a moisture barrier. Suggested applications for Uniplex 260 are:

  • plasticizer in nail lacquer
  • printing inks
  • adhesives
  • metallic and pigmented surface coatings
  • extrusion and injection molding processing aids
  • cleaning material for hot melt roll coaters.
Uniplex 260 is used when US regulations and recommendations governing food contacting applications need to be met. More information is available on request.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.262 g/ccRelative
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.28[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Melting Point 70.0 - 73.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.568
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %Karl Fischer
Shelf Life 12.0 Month
 
Descriptive Properties
Appearancewhite solid
Color<200Hazen
Content<5%di ester
 >99%Total esters

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
LyondellBasell Petrothene® LR686001 High Density Polyethylene
Lanxess Aflux® 16 Processing Aid
Ipiranga Petrochem GF 4960 HDPE
Evonik TEGOMER® DA 100 N Dispersant

PLANY9104 / 209495

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.