MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Nouryon Armeen 18D Octadecylamine
Categories: Other Engineering Material

Material Notes: Distilled primary octadecyl amine

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.784 g/cc
@Temperature 70.0 °C
 0.791 g/cc
@Temperature 60.0 °C
Solubility in Water 4.0 %
@Temperature 80.0 °C
 7.5 %
@Temperature 70.0 °C
 9.3 %
@Temperature 65.0 °C
Viscosity 39.9 cP
@Temperature 75.0 °C
 42.2 cP
@Temperature 65.0 °C
 43.7 cP
@Temperature 55.0 °C
Vapor Pressure 0.000130 bar
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.540 BTU/lb-°F
Melting Point 56.0 °C
Boiling Point 2.00 °C
@Pressure 0.0221315 MPa
 8.00 °C
@Pressure 0.0261312 MPa
 32.0 °C
@Pressure 0.0309308 MPa
 349 °C
@Pressure 0.101325 MPa
Pour Point 46.0 °C
Flash Point >= 150 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %
 
Descriptive Properties
Amine number204-213 mg KOH/g
AppearanceSolid
Content= 2 %Secondary Amine
 = 98 %Primary Amine
 0-3 g I2/100 gIodine value
 263-275 g/eqNeutralization equivalent
Equivalent mass269 g/eq
HLB8Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY185 / 285708

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.