MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nouryon Perkadox 24-W35 Dicetyl peroxydicarbonate
Categories: Other Engineering Material

Material Notes: Initiator (35% water-based emulsion) for (co)polymerization of vinyl chloride and vinylidene chloride.

CAS number: 26322-14-5

EINECS/ELINCS No.: 247-611-0

Applications: Perkadox 24-W35 is applied as an initiator in the suspension polymerization of vinylchloride in the temperature range between 45°C and 65°C. Perkadox 24-W35 may be used in combination with other peroxides such as 1,1,3,3- Tetramethylbutyl peroxyneodecanoate (Trigonox 423), Cumyl peroxyneodecanoate (Trigonox 99) or Dilauroyl peroxide (Laurox) to increase reactor efficiency. Perkadox 24-W35 is suitable for the manufacture of plastics for food contact applications. Reasons to use a water-based peroxide suspension instead of a solid or solvent-based peroxide are the following: enhanced safety, solvent free. No contamination of the VCM recycle stream, enhancement of PVC purity, easy to use (pumpable) in ‘closed reactor technology’, easy to dilute with water. Perkadox 24-W35 contains a minimum of surfactants, and these are carefully selected so as not to influence the properties of the PVC produced.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Half-life  0.100
@Temperature 84.0 °C
0.100
@Temperature 183 °F
[hr]
 1.00
@Temperature 65.0 °C
1.00
@Temperature 149 °F
[hr]
 10.0
@Temperature 48.0 °C
10.0
@Temperature 118 °F
[hr]
Viscosity 500 cP500 cP
Storage Temperature 0.000 - 15.0 °C32.0 - 59.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 40.0 °C104 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite suspension, no contamination
Assay34.0-36.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY765 / 286288

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.