MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyram PE322G22 PET, 22% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes: 22% Glass fiber reinforced, flame retardant PET for injection molding applications.

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccDIN 53479
Water Absorption 0.50 %DIN 53495
Moisture Absorption at Equilibrium 0.20 %23° C, 50% RH; DIN 53714
Linear Mold Shrinkage 0.0030 cm/cm
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 280 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 100 MPaASTM-D638
Elongation at Break 2.5 %ASTM-D638
Flexural Strength 150 MPaASTM D790
Flexural Modulus 6.70 GPaASTM-D790
Izod Impact, Notched 0.800 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmDIN 53482
Dielectric Constant 3.6
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 29.0 kV/mmVDE 0303/4
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C
Deflection Temperature at 0.46 MPa (66 psi) 250 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 226 °CDIN 53461
Flammability, UL94 V-2
@Thickness 3.00 mm
Glow Wire Test 960 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1102 UV  Polyethylene Terephthalate (PET) Glass Fiber 15% - UV Stable
E-Polymers TEKALOY® F50G30 30% Glass Fiber Reinforced PBT/PET Alloy
Covestro Makroblend® UT305 PC/PET Blend
Albis Plastics PC/PET 748/718 GF 20 HZ 20% Glass Fiber

PPOLYRA134 / 57396

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.