MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nouryon Trigonox 127 Polymer Tert-Amyl peroxybenzoate
Categories: Other Engineering Material

Material Notes: Peroxide used for (co)polymerization of styrene in the temperature range of 100-135°C.

CAS number: 4511-39-1

EINECS/ELINCS No: 224-831-5

Applications: Polymerization of styrene Trigonox 127 may be used for the (co)polymerization of styrene in the temperature range of 100-135°C. In practice, combinations of two or more peroxides with diverging activities are used to reduce the residual monomer content in the final polymer and to increase reactor efficiency. During polymerization, the temperature is increased incrementally to insure that the temperature necessary to attain the optimum properties for each peroxide is reached. In this respect, Trigonox 127 is often used with more active initiators, such as dibenzoyl peroxide (Perkadox LW75) or tert-butyl peroxy-2-ethylhexanoate (Trigonox 21S). In a mass process Trigonox 127 may be used to increase the rate of polymerization.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
Half-life  0.100
@Temperature 139 °C
0.100
@Temperature 282 °F
[hr]
 1.00
@Temperature 118 °C
1.00
@Temperature 244 °F
[hr]
 10.0
@Temperature 99.0 °C
10.0
@Temperature 210 °F
[hr]
Molecular Weight 208.3 g/mol208.3 g/mol
Storage Temperature <= 20.0 °C<= 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 60.0 °C140 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay= 94.0 %
Content= 7.22 %Active oxygen
Content (%)7.68Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1008 / 286531

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.