MARPOL® LL6F 802 is an ethylene 1-hexene LLDPE resin with good stiffness at thin gauges, good drawdown and excellent processability. This resin is suitable for blown and cast film applications and for blends with LLDPE or HDPE. Recommended Applications: Stretch wrap, overwrap, coextrusions, blown film and cast film. Additives: Antiblock – no, Slip – no. Form(s): Pellets. Information provided by Marco Polo International, LLC |