MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL™ NH7112 PPE+PS (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS)

Material Notes: NORYL™ NH7112 resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable and extrusion grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm and V1 at 1.5mm along with a UL746C Outdoor Suitability rating of F1. NORYL NH7112 resin offers an exceptional balance of strength and dimensional stability and is an excellent candidate for electrical and electronic applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Density 1.17 g/ccISO 1183
Water Absorption 0.22 %23°C/sat; ISO 62
Moisture Absorption 0.0700 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.5 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 14 g/10 min
@Load 5.00 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 83.0 MPa5 mm/min; ASTM D638
 85.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 83.0 MPa5 mm/min; ASTM D638
 85.0 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Elongation at Yield 3.0 %5 mm/min; ASTM D638
 3.0 %5 mm/min; ISO 527
Tensile Modulus 4300 MPa5 mm/min; ASTM D638
 4400 MPa1mm/min; ISO 527
Flexural Strength 134 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 137 MPa1.3 mm/min, 50 mm span; ASTM D790
 140 MPa2 mm/min; ISO 178
Flexural Modulus 3750 MPa1.3 mm/min, 50 mm span; ASTM D790
 4150 MPa2 mm/min; ISO 178
Izod Impact, Notched 70.0 J/mASTM D256
 60.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 7.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 24.0 kJ/m²80*10*4; ISO 180/1U
 26.0 kJ/m²80*10*3; ISO 180/1U
 25.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 31.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 31.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²ISO 179/2C
 7.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 15.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 3.00e+17 ohmROA; IEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
 2.93
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.0034
@Frequency 1e+6 Hz
ASTM D150
 0.0034
@Frequency 1e+6 Hz
IEC 60250
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness >=0.800 mm
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=0.800 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 137 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 138 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 148 °CRate B/50; ASTM D1525
 148 °CRate B/50; ISO 306
 150 °CRate B/120; ISO 306
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 110 °CUL 746B
Flammability, UL94 V-1
@Thickness >=0.800 mm
UL 94
 5VA
@Thickness >=2.50 mm
UL 94
Glow Wire Test 775 °C
@Thickness 1.00 mm
IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
 800 °C
@Thickness 2.00 mm
IEC 60695-2-13
 800 °C
@Thickness 2.50 mm
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 2.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 260 - 280 °CInjection Molding
Zone 1 240 - 260 °C
Zone 2 260 - 280 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 120 °C
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI14445 / 247912

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.