MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound LC00APXQ Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP THERMOCOMP LC00APXQ compound is based on Polyetheretherketone (PEEK) resin containing 50% carbon fiber. Added features of this grade include: Exceptional Processing, Electrically Conductive.

Features: High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Exceptional Processing,Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D792
Moisture Absorption 0.0300 %0.0300 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0013 - 0.0025 cm/cm0.0013 - 0.0025 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.013 cm/cm0.0060 - 0.013 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 320 MPa46400 psi5 mm/min; ISO 527
 328 MPa47600 psi5 mm/min; ASTM D638
Elongation at Break 1.1 %1.1 %5 mm/min; ISO 527
 1.2 %1.2 %5 mm/min; ASTM D638
Tensile Modulus 47.4 GPa6870 ksi1 mm/min; ISO 527
 49.8 GPa7220 ksi5 mm/min; ASTM D638
Flexural Strength 473 MPa68600 psiISO 178
 505 MPa73200 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 40.5 GPa5870 ksi1.3 mm/min, 50 mm span; ASTM D790
 40.73 GPa5907 ksi2 mm/min; ISO 178
Poissons Ratio 0.450.45ASTM E132
Shear Modulus 5.187 GPa752.3 ksiASTM D732
Shear Strength 114 MPa16500 psiASTM D732
Izod Impact Notched 77.0 J56.8 ft-lbASTM D256
Izod Impact, Unnotched 7.68 J/cm14.4 ft-lb/inASTM D4812
Dart Drop, Total Energy 7.00 J5.16 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 1000 ohm100 - 1000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 2.00 µm/m-°C
@Temperature -40.0 - 150 °C
1.11 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
CTE, linear, Transverse to Flow 20.0 µm/m-°C
@Temperature -40.0 - 150 °C
11.1 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 335 °C
@Thickness 3.20 mm
635 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 380 - 400 °C716 - 752 °F
Zone 3 380 - 400 °C716 - 752 °F
Mold Temperature 175 - 190 °C347 - 374 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Screw Speed 60 - 100 rpm60 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81676 / 289623

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.