MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Nouryon CMC WR Sodium Carboxymethylcellulose
Categories: Other Engineering Material

Material Notes: CMC WR product is a purified Sodium Carboxymethylcellulose, based on sustainably sourced cellulose.

Applications: CMC WR product is a versatile additive due to its ability to retain water, thicken liquids, regulate flow properties, suspend and stabilize dispersion and act as a film forming agent. It is a water-soluble polymer dissolving in cold as well as in warm water.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 100 - 2000 cP1% (25ºC, Brookfield LV)
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 12 %
 
Descriptive Properties
AppearanceWhite to cream powder
CMC= 96 %Sodium CMC, dry basis
Content= 4 %Sodium Chloride, dry basis
 0.70 – 0.90Degree of substitution
OdorEssentially odor free
Sieve= 4 %= 0.355 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY468 / 285991

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.