MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EOS Aluminum AlSi10Mg DMSL on EOS M 400-4; 80µm Layer Thickness
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: The HiPro process parameters offer the highest productivity of aluminum parts on the EOS M 400-4.

Main Characteristics:

  • Similar mechanical properties as casting parts
  • Up to 261 cm³/h build rate
  • Very cost efficient
  • Variable options in development
Typical Applications: AlSI10Mg is a very widely used casting alloy. This process parameter is developed specifically for fast production and similar quality as conventional produced casting parts.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Porosity 0.30 %0.30 %
Thickness 80.0 microns3.15 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 310 MPa45000 psiheat treated
 370 MPa53700 psias manufactured
Tensile Strength, Yield 220 MPa31900 psiheat treated
 230 MPa33400 psias manufactured
Elongation at Break 2.5 %2.5 %as manufactured
 6.0 %6.0 %heat treated
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 87.1 - 90.75 %87.1 - 90.75 %Balance
Copper, Cu <= 0.050 %<= 0.050 %
Iron, Fe <= 0.55 %<= 0.55 %
Lead, Pb <= 0.050 %<= 0.050 %
Magnesium, Mg 0.25 - 0.45 %0.25 - 0.45 %
Manganese, Mn <= 0.45 %<= 0.45 %
Nickel, Ni <= 0.050 %<= 0.050 %
Silicon, Si 9.0 - 11 %9.0 - 11 %
Tin, Sn <= 0.050 %<= 0.050 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.10 %<= 0.10 %
 
Descriptive Properties
Volume rate18.1 mm3/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS918 / 280578

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.