MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
High-Leaded Tin Bronze, UNS C93800, Copper Casting Alloy, M07 Temper, As Continuous Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Continuous Cast

Casting Characteristics: High – Casting Yield, Fluidity; Medium –Gassing; Low - Drossing, Effect of Section Size, Shrinkage in Solidification

Fabrication Properties: Good Suitability – Soldering; Poor Suitability – Brazing

Typical uses: Acid Resisting Applications; Backs for Lined Journal Bearings for Locomotives; Backs for Lined Journal Bearings for Passenger Cars; Bearings; Freight Car Bearings; General Service Bearings for Moderate Pressure; Industrial Centrifuges; Low Friction, Moderate Pressure Bushings; Machine Parts Pump Bodies for Acid Mine Water; Pumps; Railroad Applications; Railroad Engine Casings; Wearing Material for Rod Bushings; Wearing Material for Shoes; Wearing Material for Wedges; Large Bearings for Ships

Applicable Specifications: As Centrifugal Cast – Castings SAE J461, Castings SAE J462, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Permanent Mold Cast – Castings SAE J462, Castings SAE J461; As Sand Cast – MILITARY MIL-C-22229, Castings ASTM B763/B763M, Castings SAE J462, ASTM B66, Castings SAE J461, Castings ASTM B584; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.334 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 25.0 ksifor Standard
Tensile Strength, Yield >= 16.0 ksifor Standard, 0.5% Ext
Elongation at Break >= 5.0 %for Standard
Tensile Modulus 10500 ksi
Machinability 80 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000156 ohm-cm11% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 30.2 BTU-in/hr-ft²-°F
Melting Point 600 °FIncipient
 1570 - 1730 °F
Solidus 1570 °F
Liquidus 1730 °F
Shrinkage 1.04 %Patternmaker's Shrinkage (2/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.80 %
Copper, Cu 75 - 79 %
Iron, Fe <= 0.15 %
Lead, Pb 13 - 16 %
Nickel, Ni <= 1.0 %
Phosphorus, P <= 0.050 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.080 %
Tin, Sn 6.3 - 7.5 %
Zinc, Zn <= 0.80 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC93800x1 / 293231

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.