LEXAN JK2500 compound is based on Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend containing 20% carbon fiber. Added features of this grade include: Electrically Conductive, EMI/RFI Shielding Effectiveness of 21 dB at 1.5 mm, Non-Brominated, Non-Chlorinated Flame Retardant. Features: EMI/RFI Shielding,High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Non-Chlorinated,Non-Brominated,Electrically Conductive Information provided by SABIC |