MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Epoxies, Etc 20-2175 Polyurethane Potting Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Description: 20-2175 is a two-component and dielectric potting and encapsulating compound. This product has unique flow and rheology characteristics that allows filling of cavities with small holes where traditional materials would leak. 20-2175 was formulated for use in potting cable end assemblies, watertight electrical connectors, cables, printed circuitry, and other electrical components. It provides a quick gel to prevent too much flow.

Features:

  • Outstanding environmental performance
  • Controlled flow
  • Easy Mixing
  • Available in Triggerbond® Cartridges

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccPolyol
 1.15 g/cc1.15 g/ccIso
Viscosity 500 cP500 cPPolyol
 3000 cP3000 cPIsocyanate
Storage Temperature 24.0 - 30.0 °C75.2 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 2.0e-11 ohm2.0e-11 ohm
Dielectric Strength  >= 15.7 kV/mm
@Thickness 3.17 mm
>= 400 kV/in
@Thickness 0.125 in
 23.6 kV/mm
@Thickness 1.59 mm
600 kV/in
@Thickness 0.0625 in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Cure Time 4320 min72.0 hour
Gel Time 15.0 min15.0 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorBlack
Mix Ratio100:100Parts by volume (Polyol:Iso)
 90:100Parts by weight (Polyol:Iso)
Working Time6 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX086 / 316763

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.