MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-KON™ Compound DX96717C Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX96717C compound is based on Polycarbonate (PC) resin containing conductive carbon powder. Added features of this grade include: Electrically Conductive, Flame Retardant.

Features: Flame Retardant,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.170 %0.170 %23°C/50% RH/24 hrs; ASTM D570
 0.250 %0.250 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/in24hrs; ASTM D955
 0.0075 cm/cm0.0075 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in24hrs; ASTM D955
 0.0075 cm/cm0.0075 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 51.0 MPa7400 psiISO 527
 54.0 MPa7830 psiASTM D638
Tensile Strength, Yield 61.0 MPa8850 psiISO 527
 63.0 MPa9140 psiASTM D638
Elongation at Break 9.9 %9.9 %ASTM D638
 11.1 %11.1 %ISO 527
Elongation at Yield 4.7 %4.7 %ISO 527
 5.0 %5.0 %ASTM D638
Tensile Modulus 2.48 GPa360 ksi50 mm/min; ASTM D638
 2.70 GPa392 ksi1 mm/min; ISO 527
Flexural Strength 98.0 MPa14200 psiASTM D790
 98.0 MPa14200 psiISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
 2.89 GPa419 ksiASTM D790
Izod Impact Notched 64.0 J47.2 ft-lbASTM D256
Izod Impact, Unnotched 18.31 J/cm34.30 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 123 kJ/m²58.5 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 27.0 J19.9 ft-lbpeak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10000 - 1.00e+8 ohm10000 - 1.00e+8 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
@Thickness 3.20 mm
289 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 131 °C
@Thickness 3.20 mm
268 °F
@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.80 mm
V-0
@Thickness 0.0709 in
UL 94 by SABIC-IP
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81273 / 289220

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.