MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Zytel® RS LC1000 BK385 Nylon 1010
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion

Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. The material is flexible unreinforced UV and heat sta

Former DuPont product acquired by Celanese in 2022.

Key Words: PA1010
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccDAM; ISO 1183
Moisture Absorption 1.00 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Test 130 cm³/gISO 307 1157 1628
Linear Mold Shrinkage, Flow 0.014 cm/cmDAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmDAM; ISO 294-4 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 49.0 MPa50%RH; ISO 527-1/-2
 60.0 MPaDAM; ISO 527-1/-2
Elongation at Break 50 %DAM; Nominal; ISO 527-1/-2
 >= 50 %50%RH; Nominal; ISO 527-1/-2
Elongation at Yield 4.6 %DAM; ISO 527-1/-2
 24 %50%RH; ISO 527-1/-2
Tensile Modulus 1160 MPa50%RH; ISO 527-1/-2
 2100 MPaDAM; ISO 527-1/-2
 295 MPa
@Temperature 120 °C
50%RH; ISO 11403-1 -2
 311 MPa
@Temperature 120 °C
DAM; ISO 11403-1 -2
 886 MPa
@Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 1249 MPa
@Temperature 40.0 °C
DAM; ISO 11403-1 -2
 2388 MPa
@Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 2407 MPa
@Temperature -40.0 °C
DAM; ISO 11403-1 -2
Flexural Modulus 1740 MPaDAM; ISO 178
Charpy Impact Unnotched NBDAM; ISO 179/1eU
 NB50%RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
50%RH; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²DAM; ISO 179/1eA
 10.0 kJ/m²50%RH; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
50%RH; ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 115 µm/m-°CDAM; ISO 11359-1/-2
Melting Point 203 °CDAM; 10°C/min; ISO 11357-1/-3
Flammability, UL94 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
 HB
@Thickness 3.00 mm
DAM; IEC 60695-11-10
 
Descriptive Properties
Delivery formPellets
Part Marking Code>PA1010<ISO 11469
ProcessingOther Extrusion
 Profile Extrusion
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA1010ISO 1043
Special characteristicsHeat stabilized or stable to heat
 U.V. stabilized or stable to weather

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® Terra DS 22 natural color Nylon 1010
Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, dry
DuPont Mobility and Materials Zytel® RS LC1000 BK385 Nylon 1010 (With Extended Stress-Strain Tabular Data)
Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, conditioned
Celanese Zytel® 105F BK010 PA66

PZDSY5479 / 161306

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.