System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Celanese Zytel® 70G30REF BK314LM PA66-GF30
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 30% Glass Fiber Filled
Material Notes:
30% Glass Reinforced, Laser Markable, Polyamide 66, developed for electrical and electronics applications
Former DuPont product acquired by Celanese in 2022.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.37
g/cc
DAM; ISO 1183
Moisture Absorption
1.90 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity
120000
cP
@Shear Rate 1000 1/s,
Temperature 280 °C
Melt; ISO 11443
Viscosity Number
124
cm³/g
formic acid 90%; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow
0.0030
cm/cm
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.010
cm/cm
DAM; ISO 294-4, 2577
Mechanical Properties
Original Value
Comments
Elongation at Break
3.0 %
DAM; ISO 527-1/-2
5.0 %
50%RH; ISO 527-1/-2
130 %
50%RH; ISO 527-1/-2
190 %
DAM; ISO 527-1/-2
Tensile Modulus
7000
MPa
50%RH; ISO 527-1/-2
10000
MPa
DAM; ISO 527-1/-2
Flexural Strength
280
MPa
DAM; ISO 178
Flexural Modulus
6000
MPa
50%RH; ISO 178
9000
MPa
DAM; ISO 178
Poissons Ratio
0.34
DAM
0.35
50%RH
Charpy Impact Unnotched
50.0
kJ/m²
@Temperature -30.0 °C
50%RH; ISO 179/1eU
50.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
55.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
80.0
kJ/m²
@Temperature 23.0 °C
50%RH; ISO 179/1eU
Charpy Impact, Notched
9.00
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
10.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
11.0
kJ/m²
@Temperature 23.0 °C
50%RH; ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+11
ohm-cm
50%RH; IEC 62631-3-1
>=
1.00e+13
ohm-cm
DAM; IEC 62631-3-1
Dielectric Strength
36.0
kV/mm
50%RH; IEC 60243-1
37.0
kV/mm
DAM; IEC 60243-1
Comparative Tracking Index
600
V
DAM; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
22.0
µm/m-°C
DAM; ISO 11359-1/-2
16.0
µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
23.0
µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow
84.0
µm/m-°C
DAM; ISO 11359-1/-2
72.0
µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
146
µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Specific Heat Capacity
2.00
J/g-°C
Melt
Thermal Conductivity
0.250
W/m-K
Melt; ISO 22007-2
Melting Point
266
°C
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
258
°C
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
254
°C
DAM; ISO 75-1/-2
Glass Transition Temp, Tg
20.0
°C
10°C/min; 50%RH; ISO 11357-1/-3
75.0
°C
10°C/min; DAM; ISO 11357-1/-3
Flammability, UL94
HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
HB
@Thickness 0.400 mm
DAM; IEC 60695-11-10
Flame Spread
26.0
mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index
23 %
DAM; ISO 4589-1/-2
Processing Properties
Original Value
Comments
Melt Temperature
295
°C
Optimum
285
-
305
°C
Mold Temperature
70.0
-
120
°C
100
°C
Optimum
Ejection Temperature
210
°C
Drying Temperature
80.0
°C
Dry Time
2.00
-
4.00
hour
Dehumidified Dryer
Moisture Content
<= 0.20 %
Hold Pressure
50.0
-
100
MPa
Descriptive Properties
Additives
Low halide content
Release agent
Drying Recommended?
yes
FMVSS Class
B
ISO 3795 (FMVSS 302)
Hold pressure time
3 s/mm
ISO designation
ISO 16396-PA66,GF30,M1CGO2RW,S14-100
Part Marking Code
>PA66-GF30<
ISO 11469
Polymer
PA66-GF30
Resin Identification
PA66-GF30
Screw tangential speed
<0.2 m/s
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PDSX5327c / 296049
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.