MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® STAR S 218 V30 BLACK 31N Nylon 6, 30% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Product Description: Ultramid® STAR S 218 V30 BLACK 31N is based on a patented high flow polyamide 6 resin, heat stabilized, reinforced with 30% of glass fiber, for injection molding. Due to its outstanding flow characteristics, this grade provides a significant productivity improvement and allows more freedom in mold and part design versus a standard polyamide solutions.

Availability: Africa & Middle East; Asia Pacific; North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Heat Stabilizer

Features: Good Dimensional Stability; Good Mold Release; Heat Stabilized – Inorganic; High Flow; Outstanding Surface Finish

Uses: Consumer Applications; Furniture; General Purpose; Industrial Applications

Agency Ratings: EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA6-GF30

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Maximum Moisture Content 0.200.20
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiISO 527-2
Elongation at Break 3.5 %3.5 %ASTM D638
 3.5 %3.5 %ISO 527-2
Tensile Modulus 6.00 GPa870 ksiISO 527-1
Flexural Strength 140 MPa20300 psiASTM D790
Flexural Modulus 5.10 GPa740 ksiASTM D790
 5.30 GPa769 ksiISO 178
Izod Impact, Notched (ISO) 4.62 kJ/m²2.20 ft-lb/in²ASTM D256
 14.1 kJ/m²
@Temperature -30.0 °C
6.70 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 14.9 kJ/m²
@Temperature 22.8 °C
7.10 ft-lb/in²
@Temperature 73.0 °F
ISO 180/A
Charpy Impact Unnotched 6.93 J/cm²33.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²6.20 ft-lb/in²ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 235 °C446 - 455 °F
Middle Barrel Temperature 235 - 240 °C455 - 464 °F
Front Barrel Temperature 240 - 245 °C464 - 473 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2045 / 310738

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.