MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Konson Barium Stearate for PVC Heat Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Barium stearate

CAS No.: 6865-35-6

Molecular Fomula: C36H70BaO4

Description: Barium stearate is white fine powder, insoluble in water. When mixed with hot, strong mineral acids, they decomposed into stearic acid and corresponding barium salts. This series product has good thermo stability and processing performance, reasonable formulation. It has excellent internal and external Iubricating balance; do not need any more Iubricant. It 15 especially suitable for pressure pipes, has wide compatibility to the different feed rate and different quality padding.

Application: Used as machine high temperature resistant lubricants, rubber products of high temperature resistant additives, PVC plastic light heat stabilizer. the thermal stability of PVC products agent.a waterproofing agent, lubricant and bearing lining. high-temperature resistant powder for rubber products. It can be Used as PVC stabilizer and lubricant. In all of the alkaline earth metal stearate, it has the best heat-resistance. It is mainly used for transparent film, sheet, artificial leather and soft plate, pipe, etc. It also can be used as high- temperature stripping agent and mechanical with high temperature lubricant. heat stabilizer of vinyl chloride copolymer. It has good long-term heat resistance and lubricity, stable effect than calcium stearate, but less than lead stearate.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 75 µm>99.5%
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 210 °C
 
Component Elements PropertiesOriginal ValueComments
Barium, Ba 19.3 - 20.7 %
 
Descriptive Properties
AppearanceWhite
Content<0.5%Free Acid (stearic acid)
Loss of Drying=0.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS068 / 256113

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.