Description: Advanced-PP 1151K is a propylene homopolymer for high transparency thermoforming applications with enhanced optical appearance. The resin is nucleated and contains antistatic agent. The product provides enhanced processability Application: Thermoformed packaging for e.g. dairy products and desserts. Regulatory Information: The Grade Advanced-PP 1151K and additives incorporated comply with United States FDA Regulation 21CFR 177.1520 Olefin Polymers and European Regulation (EU) 10/2011 (and its amendments). Specific information is available upon request. Information provided by Advanced Petrochemical Company |