MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
EOS PA 2210 FR Nylon 12, Flame Retardant
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Flame Retardant

Material Notes: This white polyamide 12 powder is equipped with a halogen-free chemical flame retardant. Underwriters Laboratories (UL) has issued a Blue Card (equivalent to the well-known Yellow Card) specifically dedicated to 3D printing materials to PA 2210 FR: at wall thicknesses above 3 mm, it meets the required fire protection class UL 94 / V-0, primarily relevant for the production of electric and electronic components and applications in the aerospace and mobility sectors.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.06 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 41.0 MPaZ
 46.0 MPaXY
Elongation at Break 4.0 %
Tensile Modulus 2.30 GPaZ
 2.50 GPaXY
 
Thermal PropertiesOriginal ValueComments
Melting Point 185 °C20°C/min
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEOS908 / 280568

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.