MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATRON CMP natural Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes:
  • good heat deflection temperature
  • good chemical resistance
  • resistance against high energy radiation
  • high strength
  • high dimensional stability
  • high stiffness
  • high creep resistance
Target Industries:
  • semiconductor technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
Water Absorption 0.020 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 103.3ASTM D785
Tensile Strength at Break 13920 psiASTM D638
Tensile Strength, Yield 13980 psiASTM D638
Elongation at Break 4.2 %ASTM D638
Modulus of Elasticity 673.4 ksiASTM D638
Flexural Strength 22040 psiASTM D790
Flexural Modulus 636000 psiASTM D790
Compressive Yield Strength 5500 psi
@Strain 10 %
ASTM D695
Compressive Strength 19960 psi
@Strain 1 %
ASTM D695
Compressive Modulus 484200 psiASTM D695
Izod Impact, Notched 0.550 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.8
@Frequency 1000 Hz
DIN IEC 60250
 4.6
@Frequency 1e+6 Hz
DIN IEC 60250
Dissipation Factor 0.0011
@Frequency 1e+6 Hz
DIN IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µin/in-°FASTM E831
Melting Point 536 °FDIN EN ISO 11357
Maximum Service Temperature, Air 446 °Flong term
 500 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 239 °FISO-R 75 Method A
Deflection Temperature at 1.8 MPa (264 psi) 320 °FISO-R 75 Method B
Glass Transition Temp, Tg 194 °FDIN EN ISO 11357
Flammability, UL94 V-0
@Thickness 3.00 mm
 
Descriptive Properties
Colorbeige opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8233 / 319161

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.