MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay Chemicals CASO® TEC SOLUTION 25-29% Calcium Chloride
Categories: Ceramic; Halide; Fluid

Material Notes: CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.

REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - N°: 233-140-8/ CE - N°: 017-013-00-2

Applications: CASO liquid 25-29% is recommended for deicing asphalt and concrete surfaces that have been designed and constructed for winter condition or as antidust agent for unpaved roads. Fast melting action and cold temperature performances are two properties of CASO 25-29% that distinguish it from other deicers. These attributes stem from the ability of CASO 25-29% to release heat as it melts snow and ice. Calcium chloride is a key element in the strategies road department use to maintain roads in winter. These strategies include prewetting road salt before applying it to the road, and use as an anti-icer before or just after as storm begins.

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/cc
Molecular Weight 111 g/molanhydrous product
 
Thermal PropertiesOriginal ValueComments
Crystallization Temperature -35.1 °C
Boiling Point 110 °C
 
Descriptive Properties
AppearanceLiquid
Colorcolorless
Composition<10 g/kgSuspended solids
 0.5 g/kgCa(OH)2
 0.9 g/kgSO4
 1.4 k/kgFe
 250-290 g/kgCaCl2, Specifications
 259 g/kgCaCl2
 29.6 g/kgNaCl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WSOLV110 / 147759

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.