MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Röhm ACRYLITE® Hi-Gloss NTA-1 impact acrylic Acrylic polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: ACRYLITE® Hi-Gloss NTA-1 polymer is an opaque, amorphous, and impact-modified thermoplastic molding and extrusion compound based on polymethyl methacrylate.

Typical properties of ACRYLITE® Hi-Gloss acrylic polymers are:

  • excellent weather resistance
  • improved resistance to stress cracking
  • good melt flow rate
  • good polishability
  • impact resistance
The special properties of ACRYLITE® Hi-Gloss NTA-1 polymer are:
  • good heat resistance
  • available in a range of opaque colors
  • high melt strength
  • increased impact/break resistance and strength
Application: Used for injection molding of automotive parts.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccISO 1183
Water Absorption >= 3.0 %>= 3.0 %saturation, in Water; ISO 62
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 68.0 MPa9860 psi50 mm/min; ISO 527
Elongation at Break 10 %10 %Nominal; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.70 GPa392 ksi1 mm/min; ISO 527
Charpy Impact Unnotched 3.30 J/cm²15.7 ft-lb/in²ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C217 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 102 °C216 °FISO 75
Vicat Softening Point 110 °C230 °FB / 50; ISO 306
Glass Transition Temp, Tg 120 °C248 °FISO 11357
Glow Wire Ignition Temperature 675 °C1250 °FIEC 60695-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 250 °C428 - 482 °F
Mold Temperature 50.0 - 85.0 °C122 - 185 °FInjection Molding
Drying Temperature 100 °C212 °FPredrying
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourPredrying, Desiccant-Type Drier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9344 / 319961

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.