MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Morgan Advanced Ceramics WDS® Granulate Porextherm
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Description: WDS® Granulate is a microporous insulation material which has an extremely low thermal conductivity coefficient giving it very good insulating properties. WDS® Granulate consists of inorganic silicates. The main constituent is fumed silica; the other components are infrared opacifiers. WDS® Granulate is non-flammable and meets the requirements of DIN EN 13501-1; part 1, A1.

Application: WDS® Granulate is a free-flowing WDS® grade that offers excellent insulating properties. It is specially developed for filling insulation panels. The inorganic granules are specially modified for the filling of voids and spaces of complex geometry.

WDS® Granulate is also successfully used as insulation material in the following areas:

  • Industrial chimneys
  • Measuring instruments
  • Industrial plants
  • Insulated vessels
  • Special machinery
Advantages of WDS® Granulate:
  • Controls energy emissions, precisely
  • Reduces weight and volume
  • Increases heat retention
  • l Increases effective volume

Information provided by Morgan Advanced Materials

Key Words: Porextherm
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.110 - 0.135 g/cc0.00397 - 0.00488 lb/in³nominal
 0.130 - 0.160 g/cc0.00470 - 0.00578 lb/in³tapped, at AAW_843-00
 0.180 - 0.220 g/cc0.00650 - 0.00795 lb/in³vibration, at ASW_843-01
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0250 W/m-K
@Temperature 22.5 °C
0.174 BTU-in/hr-ft²-°F
@Temperature 72.5 °F
165 kg/m3; ASTM C177
 0.0260 W/m-K
@Temperature 50.0 °C
0.180 BTU-in/hr-ft²-°F
@Temperature 122 °F
200 kg/m3; ASTM C177
 0.0270 W/m-K
@Temperature 200 °C
0.187 BTU-in/hr-ft²-°F
@Temperature 392 °F
200 kg/m3; ASTM C177
 0.0350 W/m-K
@Temperature 400 °C
0.243 BTU-in/hr-ft²-°F
@Temperature 752 °F
200 kg/m3; ASTM C177
 0.0490 W/m-K
@Temperature 600 °C
0.340 BTU-in/hr-ft²-°F
@Temperature 1110 °F
200 kg/m3; ASTM C177
 0.0680 W/m-K
@Temperature 800 °C
0.472 BTU-in/hr-ft²-°F
@Temperature 1470 °F
200 kg/m3; ASTM C177
Maximum Service Temperature, Air <= 950 °C<= 1740 °F
 
Component Elements PropertiesMetricEnglishComments
SiC 30 %30 %
SiO2 70 %70 %
 
Descriptive Properties
Classification Temperature (°C)1000
Colorgrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics AL 1009™ Mac-A100W-Porous Aluminum Oxide Ceramic
Morgan Advanced Ceramics Cerox® 730 Thermal Ceramic
Morgan Advanced Ceramics Cera-Kote® Cement
Morgan Advanced Ceramics BTU-Block ™ Gue Thermal Ceramic
Morgan Advanced Ceramics BTU-Block ™ Flexible Thermal Ceramic

CMORF6115 / 202899

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.