MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lyanchemicals Tech EVA V4620J
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: 18% Ethylene Vinyl Acetate copolymer

Product description: EVAC V4620J is an 18% ethylene vinyl acetate copolymer resin, designed for a variety of foam molding application; manufactured by Lyanchemicals in China using Lyondellbasell high-pressure tubular process. EVAC V4620J exhibits low melting temperature, excellent processability and mechanical properties.

Applications: Foams, Shoe Soles, Injection Molding, Profile Extrusion and Compounds

Additives: Thermal Stabilizer: 300 ppm

Information provided by Lyanchemicals Tech Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.936 g/ccGB/T 1033-2010
Vinyl Acetate Content 18 %GB/T 1591-1994
Melt Flow 2.84 g/10 min
@Load 2.16 kg,
Temperature 190 °C
GB/T 3682-2000
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76ASTM D2240
Hardness, Shore D 33GB/T 2411-2008
Tensile Strength at Break 16.0 MPaGB/T 1040.2-2006
Elongation at Break 750 %GB/T 1040.2-2006
 
Thermal PropertiesOriginal ValueComments
Melting Point 89.0 °CGB/T 19466.3-2004
Vicat Softening Point 59.0 °CGB/T 1633-2000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLYANT000 / 318027

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.