MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL™ Resin GFN2F Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ GFN2F resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability. NORYL GFN2F carries a UL746C outdoor suitability rating of F1 along with FDA food contact compliance and NSF 61 listings in several colors. The properties of this material makes it an excellent candidate for water management applications such as water filter and meter components, pump housings / impellers, shower + faucet, and valves.*See NORYL GFN2 resin for NON FDA / NSF version.

Features: Hydrolytic Stability,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 300 °C
8.0 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0050 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 300 °C
9.0 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 106106ASTM D785
Tensile Strength at Break 90.0 MPa13100 psi5 mm/min; ASTM D638
 97.0 MPa14100 psi5 mm/min; ISO 527
Elongation at Break 2.5 %2.5 %5 mm/min; ISO 527
 2.6 %2.6 %5 mm/min; ASTM D638
Tensile Modulus 6.20 GPa899 ksi5 mm/min; ASTM D638
 7.07 GPa1030 ksi1 mm/min; ISO 527
Flexural Strength 160 MPa23200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 167 MPa24200 psiyield, 2 mm/min; ISO 178
Flexural Modulus 5.80 GPa841 ksi1.3 mm/min, 50 mm span; ASTM D790
 6.54 GPa949 ksi2 mm/min; ISO 178
Izod Impact Notched 119 J87.8 ft-lbASTM D256
 96.0 J
@Temperature -40.0 °C
70.8 ft-lb
@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 6.50 J/cm12.2 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²80*10*4; ISO 180/1A
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179/2C
Dart Drop, Total Energy 22.0 J16.2 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.86
@Frequency 50.0 - 60.0 Hz
2.86
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 16.5 kV/mm
@Thickness 3.20 mm
419 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor 0.00080
@Frequency 50.0 - 60.0 Hz
0.00080
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness >=1.50 mm
7.0 - 15 sec
@Thickness >=0.0591 in
UL 746A
 60 - 120 sec
@Thickness >=6.00 mm
60 - 120 sec
@Thickness >=0.236 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=1.50 mm
0.00 - 15 arcs
@Thickness >=0.0591 in
UL 746A
 15 - 30 arcs
@Thickness >=6.00 mm
15 - 30 arcs
@Thickness >=0.236 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 28.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
16.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 82.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 143 °C289 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 140 °C
@Thickness 3.20 mm
284 °F
@Thickness 0.126 in
unannealed; ASTM D648
 143 °C
@Thickness 6.40 mm
289 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °C279 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 135 °C
@Thickness 3.20 mm
275 °F
@Thickness 0.126 in
unannealed; ASTM D648
 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 143 °C289 °FRate B/50; ISO 306
 146 °C295 °FRate B/120; ISO 306
UL RTI, Electrical 90.0 °C194 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
Oxygen Index 26 %26 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 300 - 325 °C572 - 617 °F
Zone 2 275 - 320 °C527 - 608 °F
Zone 3 290 - 325 °C554 - 617 °F
Melt Temperature 300 - 325 °C572 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82318 / 290265

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.