MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Konson ZDBC Rubber Accelerator
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Zinc Dibutyl Dithiocarbamate

Molecular Formula: C18H36N2S4Zn

CAS#: 136-23-2

Properties: Relative density is 1.24g/cm3. Soluble in carbon disulfide, benzene, chloroform, insoluble in water. Storage is stable.

Applications: A fast curing accelerator for natural and synthetic rubber and latex. It is more active than rubber accelerator ZDC in dry rubber. The latex contained accelerator ZDBC can’t be prevulcanized in a week. It is an excellent activator of thiazole kinds accelerator. It can be used as antioxidant in the mixing rubber and can improve the anti-aging properties. Non color degradation, non-staining and easy dispersion in rubber process. ZDBC is regulated for use in articles in contact with food as specified under FDA 21 CFR175.105, 178.2010, 175.300, 177.1210, 177.2600 and under BgVV XXI, Categories 1-4 and ”Sonderkategorie”.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³
Molecular Weight 474.1 g/mol474.1 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 104 °C>= 219 °FInitial
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn 13 - 15 %13 - 15 %
 
Descriptive Properties
AppearanceWhite powder
Heat Loss<0.5%
Sieve residue<0.1%150µm
 <0.5%63µm
Zinc Salt Soluble in water<0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS057 / 256102

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.