System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LEXAN™ Copolymer EXL9330P Polycarbonate (PC) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
Features: High Impact Resistance
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.18
g/cc
ASTM D792
Density
1.19
g/cc
ISO 1183
Moisture Absorption
0.0200 %
Injection Molding
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
0.35 %
ISO 62-1
Viscosity
9.0
cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.0040
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse
0.0040
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
10
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
90.0
MPa
H358/30; ISO 2039-1
Tensile Strength at Break
60.0
MPa
50 mm/min; ISO 527
61.0
MPa
50 mm/min; ASTM D638
Tensile Strength, Yield
55.0
MPa
50 mm/min; ISO 527
58.0
MPa
50 mm/min; ASTM D638
Elongation at Break
125 %
50 mm/min; ISO 527
130 %
50 mm/min; ASTM D638
Elongation at Yield
6.0 %
50 mm/min; ASTM D638
6.0 %
50 mm/min; ISO 527
Tensile Modulus
2100
MPa
50 mm/min; ASTM D638
2100
MPa
1 mm/min; ISO 527
Flexural Strength
85.0
MPa
yield, 2 mm/min; ISO 178
88.0
MPa
yld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
2060
MPa
1.3 mm/min, 50 mm span; ASTM D790
2200
MPa
2 mm/min; ISO 178
Izod Impact Notched
801
J
ASTM D256
587
J
@Temperature -50.0 °C
ASTM D256
678
J
@Temperature -30.0 °C
ASTM D256
641
J
@Thickness 6.40 mm
ASTM D256
Izod Impact, Notched
1068
J/m
double-gated; SABIC method
Izod Impact, Notched (ISO)
70.0
kJ/m²
80*10*3; ISO 180/1A
80.0
kJ/m²
63.5*12.7*3.2, 23°C; ISO 180/4A
55.0
kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
65.0
kJ/m²
@Temperature -30.0 °C
63.5*12.7*3.2, 23°C; ISO 180/4A
Izod Impact, Unnotched (ISO)
NB
80*10*3; ISO 180/1U
NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
75.0
kJ/m²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
60.0
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
52.0
J
ASTM D3763
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+15
ohm
ROA; IEC 60093
Dielectric Strength
16.0
kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
17.0
kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor
0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
0.0024
@Frequency 50.0 - 60.0 Hz
ASTM D150
0.0085
@Frequency 1e+6 Hz
ASTM D150
0.0085
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
225
V
IEC 60112
Hot Wire Ignition, HWI
60
-
120
sec
UL 746A
High Amp Arc Ignition, HAI
>=
120
arcs
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
66.6
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
72.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
66.6
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
77.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test
125
°C
PASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
135
°C
Edgew 120*10*4 sp=100mm; ISO 75/Be
134
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
124
°C
Edgew 120*10*4 sp=100mm; ISO 75/Ae
120
°C
@Thickness 3.20 mm
unannealed; ASTM D648
124
°C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point
140
°C
Rate B/50; ISO 306
142
°C
Rate B/50; ASTM D1525
142
°C
Rate B/120; ISO 306
UL RTI, Electrical
125
°C
UL 746B
UL RTI, Mechanical with Impact
115
°C
UL 746B
UL RTI, Mechanical without Impact
120
°C
UL 746B
Flammability, UL94
V-1
@Thickness 0.800 mm
UL 94
V-0
@Thickness 1.49 mm
UL 94
5VA
@Thickness 2.99 mm
UL 94
Oxygen Index
35 %
ISO 4589
Glow Wire Ignition Temperature
825
°C
@Thickness 1.00 mm
IEC 60695-2-13
Glow Wire Flammability Index
960
°C
@Thickness 1.00 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Nozzle Temperature
290
-
310
°C
Zone 2
280
-
305
°C
Zone 3
295
-
315
°C
Melt Temperature
295
-
315
°C
Injection Molding
Mold Temperature
70.0
-
95.0
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
48.0
hour
Cumulative; Injection Molding
Back Pressure
0.300
-
0.700
MPa
Shot Size
40 - 60 %
Vent Depth
0.00250
-
0.00760
cm
Screw Speed
40
-
70
rpm
Descriptive Properties
UV-light, water exposure/immersion
F1
UL 746C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH80235 / 288182
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.