MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Tosoh Brownox®-X
Categories: Other Engineering Material

Material Notes: Generic Name: Manganous Manganic Oxide

Chemical Formula /Diagram: Mn3O4

Product Overview: Widely regarded for their consistent purity and particle size, these highly purified reactive compounds are in growing demand for ferrite and thermistor applications. Tosoh has supplied manganous manganic oxide to electronics parts manufacturers for ferrite magnets since 1975.

Applications: Soft ferrites; Thermistors

Information provided by Tosh Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %
 
Component Elements PropertiesOriginal ValueComments
CaO <= 0.010 %
Manganese, Mn >= 70 %
SiO2 <= 0.010 %
Sodium, Na <= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOSOH005 / 306463

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.