MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ SG-26 Silicone Grease
Categories: Fluid; Lubricant; Silicone Base; Silicone, Filled Grease

Material Notes: Thermoset SG-26 grease is a one-component silicone material used to provide heat transfer or heat dissipation between substrates. Typical applications include heat sinks in power resistors and semi-conductor devices.

Features: will not dry out or sag after long exposure to elevated temperatures. can be used on parts and devices that experience operating temperatures from -40°C to +200°C. provides high dielectric strength and excellent electrical insulation properties.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/cc
Viscosity >= 1.00e+6 cP
@Temperature 25.0 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 300 V/mil
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.220 W/m-K
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -40.0 °F
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
@Temperature 25.0 °C
from date of manufacture when stored in original, unopened container
 
Descriptive Properties
AppearanceClear Paste
Bleed %024 hours at 200 C
Weight Loss (%)0.3524 hours at 200C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMW® ELKON 100W Pure Tungsten
Röchling Polystone® PVDF FM 4910
NuSil G-9000 Silicone Grease
Overview of materials for Polyester Thermoplastic Elastomer
Lord Adhesives Thermoset™ TC-350 Thermally Conductive Silicone Grease

PLORD9230 / 232586

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.