MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
MAS Epoxies ART PRO Two-component epoxy system 100% solids
Categories: Polymer; Thermoset; Epoxy

Material Notes: MAS Art Pro epoxy resin system is a 100% solids, two-component, one to one by volume, room temperature curing epoxy resin system ideally suited for epoxy art, lacing, dirty pours and small castings. It cures to a clear, glass-like finish that resists scratching and yellowing. The system demonstrates excellent anti-blushing properties, improved UV stability and will not distort with age. Clear epoxy resin system compatible with a variety of different colorants, UV inhibitors in the formulation impart improved resistance to discoloring in the sun, Harder and more scratch resistant than other products on the market for this application.

Information provided by MAS Epoxies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccCured; ASTM D792
 8.20 lb/galHardener; ASTM D1475
Viscosity 1700 cPHardener; ASTM D2196
 3500 cPInitial Mixed; ASTM D2196
 9000 cPResin; ASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ASTM D2240
Tensile Strength 5400 psiASTM D638
Elongation at Break 5.7 %ASTM D638
Tensile Modulus 279000 psiASTM D638
Flexural Strength 8400 psiASTM D790
Flexural Modulus 242000 psiASTM D790
Compressive Strength 8000 psiASTM D695
Izod Impact, Notched 0.710 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 110 °FHDT load unknown, room temp cure; ASTM D648
 111 °FHDT load unknown, post cure; ASTM D648
Shrinkage 3.19 %ASTM D792/2196 (volumetric)
 
Processing PropertiesOriginal ValueComments
Gel Time 60.0 min150g mass; ASTM D2471
 
Descriptive Properties
ColorClear
Mix Ratio by Volume1A : 1B
Mix Ratio by Weight100A : 84
Volumetric Yield (in³/lb)25ASTM D792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASZ903 / 265518

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.