MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nouryon Trigonox 423-W50 1,1,3,3-Tetramethylbutyl peroxyneodecanoate
Categories: Other Engineering Material

Material Notes: Initiator (50% water-based emulsion) for (co)polymerization of vinyl chloride and vinylidine chloride.

CAS number: 51240-95-0

EINECS/ELINCS No: 257-077-0

Applications: Polymerization of vinyl chloride: Trigonox 423-W50 is a highly active initiator for the suspension polymerization of vinylchloride in the temperature range between 40°C and 65°C. Trigonox 423-W50 is often combined with less reactive initiators, such as peroxydicarbonates (e.g. Perkadox 16) or diacylperoxides (e.g. Laurox) to increase reactor efficiency. Reasons to use a water-based peroxide emulsion instead of a solvent-based peroxide are the following: enhanced safety, easy to use (pumpable) in ‘closed reactor technology’, easy to dilute with water

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc
@Temperature 0.000 °C
0.0336 lb/in³
@Temperature 32.0 °F
Half-life  0.100
@Temperature 76.0 °C
0.100
@Temperature 169 °F
[hr]
 1.00
@Temperature 57.0 °C
1.00
@Temperature 135 °F
[hr]
 10.0
@Temperature 40.0 °C
10.0
@Temperature 104 °F
[hr]
Brookfield Viscosity <= 2000 cP
@Temperature -10.0 °C
<= 2000 cP
@Temperature 14.0 °F
LVT, spindle #3
Molecular Weight 300.5 g/mol300.5 g/mol
Storage Temperature -20.0 - -15.0 °C-4.00 - 5.00 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 15.0 °C59.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite emulsion
Assay49.0-51.0 %
Content<1000 mg/kgInorganic + organic hydrolysable chloride
Content (%)5.32Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1121 / 286644

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.