MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ineos H02C-04 PP Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: H02C-04 is a low flow rate, high clarity, nucleated homopolymer designed for extrusion, thermoforming, blow molding, and rigid packaging applications that require good see-through clarity combined with good heat resistance. Typical applications include thermoformed cups, containers and lidding; extrusion blow molded containers and bottles, injection stretch blow molded containers and bottles, extruded sheet and profiles.
Availability: North America
Additive: Nucleating Agent
Features: Food Contact Acceptable; Homopolymer; High Clarity; Low Flow; Medium Heat Resistance; Nucleated
Uses: Blow Molding Applications; Bottles; Containers; Cups; Lids; Profiles; Rigid Packaging; Sheet; Thermoforming applications
Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520© 3.1a
RoHS Compliance: Contact Manufacture
Forms: Pellets
Processing Method: Blow Molding; Extrusion; Extrusion Blow Molding; Injection Stretch Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming

Information provided by INEOS Olefins & Polymers USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.911 g/ccASTM D792
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D785
Tensile Strength at Break 2700 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 5300 psi2.0 in/min; ASTM D638
Elongation at Break 100 %2.0 in/min; ASTM D638
Elongation at Yield 9.7 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 233000 psiASTM D790A
Izod Impact, Notched 1.20 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 3.09 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 230 °FUnannealed; ASTM D648
Vicat Softening Point 309 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 31 %
@Thickness 1.27 mm
ASTM D1003
Gloss 96 %60°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINEOSA005 / 268241

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.