System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC NORYL GTX™ Resin GTX202 Polyphenylene Ether + PA (PPE+Nylon) (Americas)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Polyphenylene Ether/PPO
Material Notes:
NORYL GTX™ 202 resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits excellent chemical resistance and excellent paintability.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.08
g/cc
ASTM D792
Density
1.09
g/cc
ISO 1183
Water Absorption
0.40 %
@Time 86400 sec
ASTM D570
Moisture Absorption
0.0700 %
Injection Molding
0.200 %
23°C/50% RH/24 hrs; ASTM D570
0.570 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
2.02 %
ISO 62-1
3.6 %
ASTM D570
Viscosity
12
cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.0103
cm/cm
24hrs; ASTM D955
0.0103
cm/cm
24hrs; ISO 294
0.011
-
0.015
cm/cm
annealed 130C 1hr; ASTM D955
0.0090
-
0.012
cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse
0.0112
cm/cm
24hrs; ASTM D955
0.0112
cm/cm
24hrs; ISO 294
0.0080
-
0.011
cm/cm
@Thickness 3.20 mm
SABIC method
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
118
ASTM D785
Tensile Strength at Break
52.0
MPa
5 mm/min; ASTM D638
54.0
MPa
5 mm/min; ISO 527
56.0
MPa
50 mm/min; ASTM D638
Tensile Strength, Yield
59.0
MPa
50 mm/min; ASTM D638
Elongation at Break
38 %
5 mm/min; ASTM D638
46 %
5 mm/min; ISO 527
52 %
50 mm/min; ASTM D638
Elongation at Yield
9.0 %
50 mm/min; ASTM D638
Tensile Modulus
2173
MPa
5 mm/min; ASTM D638
2154
MPa
@Temperature 120 °C
1 mm/min; ISO 527
Flexural Strength
89.0
MPa
yld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus
2120
MPa
1.3 mm/min, 50 mm span; ASTM D790
2227
MPa
2 mm/min; ISO 178
2240
MPa
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched
167
J
ASTM D256
53.0
J
@Temperature -40.0 °C
ASTM D256
117
J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched
NB
ASTM D4812
3204
J/m
@Temperature -40.0 °C
ASTM D4812
3204
J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO)
18.0
kJ/m²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
<= NB
80*10*4; ISO 180/1U
Charpy Impact Unnotched
<= NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
19.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
46.0
J
peak; ASTM D3763
19.0
J
@Temperature -40.0 °C
peak; ASTM D3763
36.0
J
@Temperature -30.0 °C
peak; ASTM D3763
Taber Abrasion, mg/1000 Cycles
19
CS-17, 1 kg; ASTM D1044
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
90.0
µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
93.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM E831
CTE, linear, Transverse to Flow
93.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi)
154
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
155
°C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
113
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
127
°C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point
166
°C
Rate B/50; ISO 306
167
°C
Rate B/50; ASTM D1525
232
°C
Rate A/50; ASTM D1525
235
°C
Rate A/50; ISO 306
Processing Properties
Original Value
Comments
Nozzle Temperature
275
-
300
°C
Zone 2
265
-
300
°C
Zone 3
270
-
300
°C
Melt Temperature
275
-
300
°C
Injection Molding
Mold Temperature
65.0
-
95.0
°C
Drying Temperature
95.0
-
105
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
8.00
hour
Cumulative; Injection Molding
Moisture Content
0.020 %
minimum
Back Pressure
0.300
-
1.40
MPa
Shot Size
30 - 50 %
Vent Depth
0.00130
-
0.00380
cm
Screw Speed
20
-
100
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH82113 / 290060
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.