MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY C7410 PC+ABS (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate (PC)

Material Notes: CYCOLOY C7410 resin is a talc-filled PC+ABS, nonhalogenated FR for thin wall molding applications.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D 792
Density 1.22 g/ccISO 1183
Moisture Absorption 0.0600 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.26 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 260 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 13.4 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 38.0 MPa5 mm/min; ISO 527
 44.0 MPaType I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 54.0 MPaType I, 5 mm/min; ASTM D 638
 58.0 MPa5 mm/min; ISO 527
Elongation at Break 74 %Type I, 5 mm/min; ASTM D 638
 78 %5 mm/min; ISO 527
Elongation at Yield 3.5 %Type I, 5 mm/min; ASTM D 638
 3.6 %5 mm/min; ISO 527
Tensile Modulus 3300 MPa5 mm/min; ASTM D 638
 3340 MPa1 mm/min; ISO 527
Flexural Yield Strength 95.0 MPa2 mm/min; ISO 178
 96.0 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 3180 MPa1.3 mm/min, 50 mm span; ASTM D 790
 3260 MPa2 mm/min; ISO 178
Izod Impact, Notched 71.0 J/m
@Temperature -30.0 °C
ASTM D 256
 315 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 31.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 80.0 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
 87.0 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
Vicat Softening Point 103 °CRate B/50; ASTM D 1525
 103 °CRate B/50; ISO 306
 106 °CRate B/120; ISO 306
Flammability, UL94 5VBUL 94
 V-0
@Thickness 0.800 mm
UL 94

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Mitsubishi Iupilon® MB 8700 PC/ABS
Trinseo CALIBRE™ 7100-15 Polycarbonate
Overview of materials for Polycarbonate, Molded

PSABI47624 / 188709

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.