MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ LG9000 PC+ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: PC/ABS low gloss.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Water Absorption 0.10 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.40 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 17 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Yield 54.0 MPa50 mm/min; ASTM D638
Elongation at Break 75 %50 mm/min; ASTM D638
Flexural Yield Strength 84.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 534 J/mASTM D256
 320 J/m
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 40.0 JASTM D3763
 33.0 J
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 30 - 60 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
Thermal Conductivity 0.200 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 123 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 129 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 110 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 129 °CRate B/50; ASTM D1525
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.49 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Gloss 30 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 300 °CInjection Molding
Zone 1 250 - 290 °C
Zone 2 255 - 295 °C
Zone 3 260 - 300 °C
Melt Temperature 275 - 300 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10754 / 244221

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.