MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LEXAN™ FR Resin BM5225Y Polycarbonate + ABS (PC+ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: LEXAN™ BM5225Y Polycarbonate resin is an injection moldable non chlorinated/brominated mineral-filled flame retardant grade. It features high modulus, good flow, ductility and low warpage. It has a UL94 V0@1.5mm and 5VB@1.5mm flame rating and is a good candidate for thin wall applications.

Features: Flame Retardant,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/ccASTM D792
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 3.20 mm
0.0030 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 260 °C
12 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109109ASTM D785
Tensile Strength at Break 30.0 MPa4350 psi5 mm/min; ISO 527
 34.0 MPa4930 psi5 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa7980 psi5 mm/min; ASTM D638
 56.0 MPa8120 psi5 mm/min; ISO 527
Elongation at Break 5.0 %5.0 %5 mm/min; ASTM D638
 5.0 %5.0 %5 mm/min; ISO 527
Elongation at Yield 2.8 %2.8 %5 mm/min; ASTM D638
 2.8 %2.8 %5 mm/min; ISO 527
Tensile Modulus 5.57 GPa808 ksi1 mm/min; ISO 527
 5.85 GPa848 ksi5 mm/min; ASTM D638
Flexural Strength 98.0 MPa14200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 98.0 MPa14200 psiyield, 2 mm/min; ISO 178
Flexural Modulus 6.01 GPa872 ksi1.3 mm/min, 50 mm span; ASTM D790
 6.15 GPa892 ksi2 mm/min; ISO 178
Izod Impact Notched 50.0 J36.9 ft-lbASTM D256
 37.0 J
@Temperature -30.0 °C
27.3 ft-lb
@Temperature -22.0 °F
ASTM D256
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 20.0 J14.8 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 34.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
18.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 69.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.3 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
@Thickness 3.20 mm
199 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C189 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 85.0 °C
@Thickness 3.20 mm
185 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 98.0 °C208 °FRate B/50; ASTM D1525
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-1
@Thickness >=0.800 mm
V-1
@Thickness >=0.0315 in
UL 94
 V-0
@Thickness >=1.20 mm
V-0
@Thickness >=0.0472 in
UL 94
 5VB
@Thickness >=1.50 mm
5VB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 300 °C536 - 572 °F
Zone 2 260 - 280 °C500 - 536 °F
Zone 3 270 - 290 °C518 - 554 °F
Melt Temperature 270 - 300 °C518 - 572 °FInjection Molding
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 90.0 - 105 °C194 - 221 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 16.0 hour16.0 hourCumulative; Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80480 / 288427

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.