MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ATI Allegheny Ludlum Type 441 Alloy Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stabilized with columbium and titanium to provide good weld ductility and resistance to intergranular corrosion in the weld heat affected zone.

Type 441 alloy has very good resistance to progressive scaling in both continuous and cyclic oxidizing laboratory test environments. Type 441 is weldable using traditional tungsten inert gas and metal arc inert gas procedures commonly used with stainless steel. When a filler wire is required, a matching Type 441 chemistry electrode can be used with the alloy to maintain compatible corrosion and oxidation resistance in the weld area. It is suggested that hydrogen not be mixed with inert gas (unless post weld annealing is planned) because ferritic stainless steels are subject to hydrogen embrittlement.

Information provided by Allegheny Ludlum Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.711 g/cc0.2786 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8484typical
Tensile Strength, Ultimate 510 MPa74000 psiTypical
Tensile Strength, Yield 331 MPa48000 psiTypical
Elongation at Break 29 %29 %typical in 2" (50 mm)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000587 ohm-cm0.0000587 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.20 µm/m-°C
@Temperature 20.0 - 100 °C
5.11 µin/in-°F
@Temperature 68.0 - 212 °F
 10.3 µm/m-°C
@Temperature 20.0 - 300 °C
5.72 µin/in-°F
@Temperature 68.0 - 572 °F
 10.6 µm/m-°C
@Temperature 20.0 - 500 °C
5.89 µin/in-°F
@Temperature 68.0 - 932 °F
 10.8 µm/m-°C
@Temperature 20.0 - 700 °C
6.00 µin/in-°F
@Temperature 68.0 - 1290 °F
 11.3 µm/m-°C
@Temperature 20.0 - 800 °C
6.28 µin/in-°F
@Temperature 68.0 - 1470 °F
 11.9 µm/m-°C
@Temperature 20.0 - 900 °C
6.61 µin/in-°F
@Temperature 68.0 - 1650 °F
Maximum Service Temperature, Air 1010 °C1850 °FContinuous service
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.050 %0.050 %
Carbon, C 0.020 %0.020 %
Chromium, Cr 18 %18 %
Iron, Fe 79 %79 %as balance
Manganese, Mn 0.33 %0.33 %
Nickel, Ni 0.32 %0.32 %
Niobium, Nb (Columbium, Cb) 0.69 %0.69 %
Nitrogen, N 0.021 %0.021 %
Phosphorus, P 0.025 %0.025 %
Silicon, Si 0.39 %0.39 %
Sulfur, S 0.0020 %0.0020 %
Titanium, Ti 0.27 %0.27 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy
AK Steel 441 Ferritic Stainless steel
Overview of materials for T 400 Series Stainless Steel
Type 441 Ferritic Stainless Steel, UNS S44100 (Composition Spec)
AK Steel 400 Ferritic Stainless steel

NL441 / 17950

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.