MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound DC0041PQ Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DC0041PQ compound is based on Polycarbonate (PC) resin containing 20% carbon fiber. Added features of this grade include: Electrically Conductive, Non-Brominated, Non- Chlorinated Flame Retardant, Exceptional Processing.

Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Non-Chlorinated,Non-Brominated,Exceptional Processing,Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
Moisture Absorption 0.0500 %0.0500 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0036 cm/cm0.0036 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 185 MPa26800 psi5 mm/min; ASTM D638
Elongation at Break 1.5 %1.5 %5 mm/min; ASTM D638
Tensile Modulus 21.0 GPa3050 ksi5 mm/min; ASTM D638
Flexural Strength 260 MPa37700 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 18.0 GPa2610 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 70.0 J51.6 ft-lbASTM D256
Izod Impact, Unnotched 5.00 J/cm9.37 ft-lb/inASTM D4812
Dart Drop, Total Energy 10.0 J7.38 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.19e+6 ohm-cm3.19e+6 ohm-cmASTM D257
Surface Resistance 1.40e+6 ohm1.40e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
7.78 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 35.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
19.4 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
@Thickness 3.20 mm
187 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-1
@Thickness >=0.700 mm
V-1
@Thickness >=0.0276 in
UL 94
 V-0
@Thickness >=0.800 mm
V-0
@Thickness >=0.0315 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 275 - 300 °C527 - 572 °FInjection Molding
Mold Temperature 60.0 - 85.0 °C140 - 185 °F
Drying Temperature 70.0 °C158 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 63 rpm30 - 63 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81494 / 289441

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.