MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Angst+Pfister APSOplast® PEEK GF 30 PEEK + 30% glass fibre
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: This material type, reinforced with 30% glass fibre, has a higher rigidity and creep resistance than non-reinforced PEEK and has much better dimensional stability. It is well-suited for use in parts which are exposed to high and static loads at high temperatures. Because the glass fibres tend to result in abrasion of the mating surface, the suitability of this material for slide bearings must be carefully checked for each specific application.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³DIN EN ISO 1183-1
Water Absorption  0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
DIN EN ISO 62
 0.030 %
@Time 346000 sec
0.030 %
@Time 96.0 hour
DIN EN ISO 62
Moisture Absorption 0.140 %0.140 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8989DIN EN ISO 868
Ball Indentation Hardness 250 MPa36300 psiDIN EN ISO 2039-1
Tensile Strength, Yield 80.0 MPa11600 psiDIN EN ISO 527
Elongation at Break 5.0 %5.0 %DIN EN ISO 527
Modulus of Elasticity 6.00 GPa870 ksiDIN EN ISO 527
Charpy Impact Unnotched 3.30 J/cm²15.7 ft-lb/in²DIN EN ISO 179-1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 50 Hz
3.2
@Frequency 50 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243
Dielectric Loss Index 0.0010
@Frequency 50 Hz
0.0010
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear  30.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 140 °F
 40.0 µm/m-°C
@Temperature 23.0 - 150 °C
22.2 µin/in-°F
@Temperature 73.4 - 302 °F
Thermal Conductivity 0.430 W/m-K2.98 BTU-in/hr-ft²-°F
Melting Point 343 °C649 °FISO 11357-3
Maximum Service Temperature, Air 250 °C482 °Flong term
 310 °C590 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 315 °C599 °FDIN EN ISO 75 / A
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in
 
Descriptive Properties
Colornatural (brownish grey)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP063 / 250561

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.