MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Polikim EFALON® B-40 PTFE, 40% Bronze Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearings, piston rings, valve sets, valve components.

Information provided by Polikim Polimer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.05 - 3.15 g/ccASTM D792
Deformation 1.1 - 1.2 %
@Temperature 150 °C,
Time 86400 sec,
Pressure 0.981 MPa
total
 1.4 - 2.1 %
@Temperature 23.0 °C,
Time 86400 sec,
Pressure 13.7 MPa
permanent; ASTM D621
 3.8 - 4.9 %
@Temperature 23.0 °C,
Time 86400 sec,
Pressure 13.7 MPa
total; ASTM D621
 10 - 11 %
@Temperature 150 °C,
Time 86400 sec,
Pressure 4.90 MPa
total
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64 - 68ASTM D2240
Tensile Strength, Ultimate 150 - 280 kg(f)/cm²ASTM D638
Elongation at Break 120 - 280 %ASTM D638
Compressive Strength 100 - 105 kg(f)/cm²1% Deformation; ASTM D695
Izod Impact, Notched (ISO) 11.0 - 12.0 kJ/m²ASTM D256
Coefficient of Friction 0.12
Coefficient of Friction, Static 0.060
Limiting Pressure Velocity 0.00409 - 0.00441 MPa-m/sec3 m/min
 0.00572 - 0.00621 MPa-m/sec30 m/min
 0.00654 - 0.08175 MPa-m/sec300 m/min
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+8 ohm-cmASTM D257
Surface Resistance >= 1.00e+10 ohm50% rel. humidity; ASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 - 95.0 µm/m-°C
@Temperature 25.0 - 100 °C
ASTM D696
 95.0 - 110 µm/m-°C
@Temperature 25.0 - 200 °C
ASTM D696
 125 - 135 µm/m-°C
@Temperature 25.0 - 300 °C
ASTM D696
Thermal Conductivity 0.00170 - 0.00200 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 270 °Ccontinuous
Minimum Service Temperature, Air -260 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® PA3540LT 10% Carbon Fiber, 30% Bronze, PTFE Filled Compound
Isoflon PTFE + 40% Bronze Polytetrafluoroethylene with 40% Bronze
AGC Fluon® RA3540 10% Carbon Fiber, 30% Bronze, PTFE Filled Compound
3M Dyneon™ CC144/S PTFE, 40% Bronze Filled
Total PPH 11012 Polypropylene Homopolymer, Injection Molding

PPOLIK006 / 99816

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.