MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CAB-O-SILĀ® LM-150D Fumed Silica
Categories: Other Engineering Material

Material Notes: Product highlights: CAB-O-SIL LM-150D fumed silica, the densed form of CAB-O-SIL LM-150 fumed silica, is a low surface area fumed silica which provides moderate increase in viscosity and reinforcement of sealants and rubbers. The bulk density of CAB-O-SIL LM-150 fumed silica has been mechanically increased for faster incorporation and ease of handling. All untreated fumed silicas are characterized by:
  • high purity
  • aggregated structure
  • submicron particle size
  • low bulk density
  • hydrophilic surface chemistry
Key applications: CAB-O-SIL LM-150D fumed silica is widely used to provide thixotropy and reinforcement of sealants and reinforcement in silicone rubbers. With use of a densed, higher bulk density, silica such as CAB-O-SIL LM-150D fumed silica, using very high shear dispersion equipment is recommended to achieve adequate dispersion of the silica. The higher bulk density of CAB-O-SIL LM-150D fumed silica facilitates faster wet-in or incorporation into these viscous polymer systems.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT084 / 315819

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.